Here, we come to discuss all issues related to magnet wire stripping technology, of course, first we have a clear understanding of the type of magnet wire. Enameled wire material according to different classified into three categories: copper enameled wire, aluminum enameled wire, copper clad aluminum wire. According to temperature levels (ie heat level) sub: Y (90 ℃), A (105 ℃), E (120 ℃), B (130 ℃), F (155 ℃), H (180 ℃), H + ( 200), C (220); based paint species, function, shape, weldability market is divided into: acetal wire, polyester wire, epoxy wire, polyimide wire, polyamide imide wire , polyurethane cable, self-adhesive wire, polyester-imide wire, composite enameled wire, nylon line, anti-corona wire, magnetic wire, self-lubricating wire, enameled flat wire, enamelled conductors, copper clad aluminum wire, etc.. Variety, so dizzying.
In this case, have also increased our R & D difficulty stripping enameled wire. Direct welding by hand from scratch to the paint machine to paint remover, and many, but the main objectives are: stripping - solder.
Straight line at low temperature solder to make of this we do not, mainly for 130,155,180,200,220 class can not be straight welding line. With the advances in chemical technology and the implementation of ROHS standards for improving the efficiency of stripping is the most suitable plant: enameled wire stripper (also known as stripping water, stripping water, stripping agent, paint remover).
That is the case, enameled wire stripper, they must meet the following requirements:
1, in line with ROHS standard limit: The detection unit testing companies, SGS is based.
2, obtained after stripping the copper wire, aluminum wire must be bright, rust, easy to weld. (Currently off the market, there is a high temperature powder paint stripping line, only Dongguan Bonthe BT-enameled aluminum wire stripping powder to achieve bright as a mirror, other manufacturers of serious corrosion of aluminum wire, aluminum wire after stripping the corrosion had changed dark, pitting, rough, serious impact on welding or welding wire solder layer and the natural detachment, open circuit.)
3, stripping speed, less damage on the human body.
Enameled wire stripping is also due to the matrix, the different temperature levels to choose a different magnet wire stripper:
Species Heat resistance Selected types of paint remover Stripping the required temperature Stripping time Copper magnet wire 130、155 BT-Quick enameled wire stripper 15℃-35℃ 10-45 Second 180、200、220 BT-High temperature magnet wire stripper 15℃-35℃ 1-5 Minute Or≥5 Minute BT-Enameled paint stripping powder 280-300℃ 5-45 Second Aluminum magnet wire 130、155、180、 BT—Aluminum magnet wire stripper 15℃-35℃ 1-5 Minute Or≥5 Minute 130、155、180、200、220 BT-Enameled paint stripping powder 280-300℃ 5-45 Second Copper clad aluminum wire 130、155、180、 BT—Aluminum magnet wire stripper 15℃-35℃ 1-5 Minute Or≥5 Minute 130、155、180、200、220 BT-Enameled paint stripping powder 280-300℃ 5-45 Second Rules Off with a stripper who can not afford to or more than technological requirements, and on the choice of paint stripping powder.
Related Articles
![]()
Company |
Contact us |
Friendly Link |
bont Chemical Co., Ltd
Copyright © 2004-2014,bont.cn All right reserved. 0769-23176555
All rights reserved © bont Surface-Treatment Material Co., Ltd
MII record:guangdong ICP prepared No.11029672